Skip to main content
. 2010 Sep 2;6(1):22. doi: 10.1007/s11671-010-9756-1

Figure 10.

Figure 10

a TEM image of gelatin-AgNPs synthesized at 90°C (Cgelatin: 0.4 wt%, VAgNO3: 2 mL); b XRD of gelatin-AgNPs power obtained from the sample in a; c TEM image of gelatin-AgNPs synthesized at 90°C (Cgelatin: 0.4 wt%, VAgNO3: 4 mL). AgNO3 was added in gelatin solution in two times. At first, 0.2 mL AgNO3 was added. The other AgNO3 was added into reaction mixture after 10 h.