TEM analysis of the colloidal solution. A transmission electron micrograph of the stock solution of CdSe/CdS nanorods dissolved in toluene, deposited on copper grid coated with a thin amorphous carbon film, after solvent evaporation. The average rod diameter and length, as determined by TEM were 4 and 20 nm (aspect ratio 5), respectively.