Skip to main content
. 2010 Dec 15;133(4):1016–1032. doi: 10.1021/ja1090832

Figure 2.

Figure 2

TEM image of Pt nanoparticles of 2−4 nm on the surface of Pt-CaCu3Ti4O12, following photoreduction of H2PtCl6 in 1% MeOH solution in the presence of CaCu3Ti4O12 under UV light. The scale bar is 5 nm.