Skip to main content
. 2011 Sep 3;12(4):1136–1143. doi: 10.1208/s12249-011-9682-2

Fig. 3.

Fig. 3

Particle size and span values of nitrendipine nanocrystals as a function of precipitation temperature. PVA (2.5 mg/ml) was used as stabilizer and homogenized for 20 cycles at 1,000 bar (mean ± SD, n = 3)