Figure 7.

Figure 7.

CV of 3.56 × 10−4 M anthracene at bare/GCE (curve a), AgNPs/GCE (curve b), AuNPs/GCE (curve c), Ag-AuNPs/GCE (curve d), PPyox/GCE (curve e) and PPyox/Ag-AuNPs/GCE (curve f) in acetonitrile and 0.1 M LiClO4 at a scan rate of 100 mV s−1.