Table 3.
Tensile strength and elastic modulus of the films after curing
Film | Tensile strength (MP) | Elastic modulus (MPa) |
---|---|---|
IPA | 3.70±1.2 | 393.0±32.4 |
IPA+10% PEG 400 | 3.40±1.6 | 204.6±19.9 |
IPA+20% PEG 400 | 0.12±0.06 | 1.9±1.1 |
Aq | 2.54±0.98 | 290.0±21.1 |
Aq+10% PEG 400 | 1.87± 0.45 | 164.4±17.2 |
Aq+20% PEG 400 | 2.30±1.09 | 8.8±1.4 |
IPA+10% TEC | 2.30±0.87 | 305.5±25.1 |
IPA+20% TEC | 0.53±0.16 | 15.1±3.7 |
Aq+10% TEC | 1.83±0.26 | 255.3±15.1 |
Aq+20% TEC | 2.50±1.21 | 117.0±25.0 |