Skip to main content
. 2011 Dec 13;2011:378034. doi: 10.1155/2011/378034

Figure 5.

Figure 5

Tangent modulus of a range of fibrin gel produced with varying fibrinogen concentrations. Fibrin gels were made by mixing fibrinogen (3, 10, and 30 mg/mL) with thrombin (1 μl/mL). Tensile testing of the gels was performed using a Bose ElectroForce 3200 (a–c). The tangent moduli were calculated from the slope of the plot of stress versus strain at 20% strain (n = 6) (d).