Scheme 2.

Scheme 2

Electrochemical preparation of nanoparticles. Polypyrrole was formed at constant current until 4.5 C/cm2 of current density was achieved from a 0.15 M pyrrole in 0.1 M KClO4 solution. Incubation of the film in 1 mM K2PdCl4 solution overnight exchanges perchlorate for tetrachloropalladate, which is reduced by polypyrrole to Pd0 in the film. The Pd nanoparticles were used for dechlorination (RX → RH + X) in the presence of hydrogen.