Skip to main content
. Author manuscript; available in PMC: 2012 Jan 5.
Published in final edited form as: Proc SPIE Int Soc Opt Eng. 2010;7646:764616. doi: 10.1117/12.847701

Figure 2.

Figure 2

(a) The PEDOT: PSS solution is poured onto Foam tape with PU adhesion layer in between (b) After 24 hours, the PEDOT: PSS is dried on the foam (c) The dried PEDOT: PSS is further processed by laser cutting and pattern is standard bone shape.