Figure 8.

Figure 8

Shrinkage stress versus methacrylate conversion of EBPADMA (1), PETMP-HDY-EBPADMA 2:1:2.7 (3), PETMP-HDE-EBPADMA 1.5:1.5:2.7 (4); and versus yne conversion of PETMP-HDY 2:1 (2). The systems were initiated with 1 wt% Irgacure 184, and cured by 365nm light at 10mW/cm2.