Table 1.

EOF mobility, μeo, of PDMS and quartz glass after different surface treatments

Surface derivatizationa μeo×10−4 [cm2(Vs)−1]
EOF reductionb [%]
PDMS Quartz PDMS Quartz
Uncoated 2.1±0.33 3.15±0.68 0 0
PLL-PEG (static) 0.36±0.05 0.38±0.08 83 88
PLL-PEG (dynamic) −0.76±0.23 n.a. Anodic EOF n.a.
DDM/MC (dynamic) 0.13±0.02 0.28±0.09 94 91
F108 (dynamic) 0.14±0.02 0.26±0.06 93 92
a

PDMS surfaces were plasma oxidized before surface derivatization

b

Reduction is calculated relative to uncoated surfaces