Skip to main content
. Author manuscript; available in PMC: 2013 Jan 1.
Published in final edited form as: Mech Mater. 2012 Jan 1;44:93–98. doi: 10.1016/j.mechmat.2011.07.016

Figure 6.

Figure 6

Phase Angle significantly decreased with increasing frequency in both degenerate and nondegenerate groups at 10% strain. * = p<0.05 with respect to phase angle at 10% strain at 0.01Hz. Error bars represent standard deviation.