Published in final edited form as: Biomaterials. 2011 Dec 22;33(8):2473–2481. doi: 10.1016/j.biomaterials.2011.12.005

Table 1.

Feeding ratios of monomer MAETAC to monomer PEGMA in the prepolymerization solutions for the preparation of hydrogel samples and elemental analysis of these samples. The prepared hydrogel samples showed different appearance according to the feeding ratio of the two monomers.

Hydrogel
Names
Ratio of MAETAC to PEGMA
Elemental Analysis
Final Gel
Appearance
v/v w/w n/n % C % H % N
HS-1 9.00 6.77 11.74 40.93 9.10 4.55 Clear
HS-2 4.00 3.01 5.22 42.94 9.09 4.21 White
HS-3 2.33 1.76 3.04 44.15 8.96 3.74 White
HS-4 1.50 1.13 1.96 46.17 9.06 3.35 White
HS-5 1.00 0.75 1.30 48.65 9.11 3.00 White
HS-6 0.67 0.50 0.87 49.35 8.93 2.34 White
HS-7 0.43 0.32 0.56 49.64 8.86 1.74 White
HS-8 0.25 0.19 0.33 50.97 8.77 1.19 White
HS-9 0.11 0.08 0.14 52.79 8.51 0.63 Clear
HS-10 0.05 0.04 0.07 54.30 8.15 0.29 Clear
HS-11 0.01 0.01 0.01 54.39 8.16 <0.05 Clear

Note the elemental composition of MAETAC (C9H18NO2Cl, Mw = 207.7) is as follows: C: 52.0%; H: 8.7%; and N: 6.7%. v/v, w/w, and n/n stand for the volume ratio, mass ratio and molar ratio of MAETAC monomer to PEGMA monomer, respectively.