Skip to main content
. 2012 Jan 12;2012:310702. doi: 10.1155/2012/310702

Figure 2.

Figure 2

Shows a mixed fracture interface surface (mode 4). The dentinal surface is sealed and cracks propagate through the luting cement (arrows).