Skip to main content
. Author manuscript; available in PMC: 2013 Jan 6.
Published in final edited form as: Macromolecules. 2012 Jan 6;45(2):1062–1069. doi: 10.1021/ma202098s

Figure 7.

Figure 7

Quasi-static tensile testing-to-failure results for samples with increased supramolecular cross-linking. Failure strain decreases while failure stress increases with increased UPy content (upper, a). Toughness peaks around 15 wt % UPy. All tests were conducted at the peak of loss modulus from DMA (1 Hz) (middle, b). Peak of loss modulus as determined by DMA at 1 Hz for samples that were subsequently quasi-statically strained to failure (lower, c).