Skip to main content
. Author manuscript; available in PMC: 2013 Jan 1.
Published in final edited form as: Macromolecules. 2012 Jan 1;45(1):39ā€“45. doi: 10.1021/ma202282p

Figure 2.

Figure 2

Nanogel erosion via cross-link scission occurs in presence of DTT (red) or cysteine (blue), monitored in situ via MALS. Error bars (black) represent one standard deviation about the mean of measurements.