Skip to main content
. 2012 Feb 3;2:247. doi: 10.1038/srep00247

Figure 5. Comparison of the ErGO-DLCs prepared by electrodepositing ErGO for different time.

Figure 5

(a) Plots of impedance phase angle versus frequency. (b) Evolutions of the imaginary parts of the specific capacitances versus frequency. (c) Plots of Cs versus frequency.