Skip to main content
. Author manuscript; available in PMC: 2013 Mar 1.
Published in final edited form as: Acta Biomater. 2011 Dec 13;8(3):1109–1116. doi: 10.1016/j.actbio.2011.12.005

Figure 3.

Figure 3

SEM images of surface-induced nanocomposites formed on SAMs with various terminal groups. The mineralization was conducted for 24 h. The nanocomposites formed on unmodified gold surface (Au) and polystyrene surface (PS) were used for comparison. The scale bar is 200 nm.