Complex viscosity of the myocardial matrix material at 25°C for frequencies from 0.1-50 Hz.

Condition k n r2
6mg/ml
Standard 0.1300 -0.466 0.955
0.5× PBS 0.1548 -0.523 0.959
1.5× PBS 0.1580 -0.519 0.963
pH 8.5 0.2030 -0.550 0.978
8mg/ml
Standard 0.4976 -0.617 0.982
0.5× PBS 0.4402 -0.656 0.994
1.5× PBS 0.4641 -0.580 0.983
pH 8.5 0.4568 -0.606 0.988