Skip to main content
. 2009 Jan 19;9(1):556–567. doi: 10.3390/s90100556

Figure 7.

Figure 7.

Statistical forecast of the dominant cracks at failure. Top row: micro-structure A; bottom row: micro-structure B. Left column: perfect GBs ( tGM=2.5 GPa, tGBM=2.5 GPa); right column: defective GBs ( tGM=2.5 GPa, tGBM=2.0 GPa).