Skip to main content
. 2010 May 19;2(6):1594–1600. doi: 10.1021/am100050v

Figure 5.

Figure 5

Plot of stress monitoring over time (+) of a polymer film held under constant strain (1%) while cycling UV irradiation (365 nm) at 2 min intervals. The temperature measured by the DMA over this time scale is plotted on the second y-axis (•).