Heat treatment changes the morphology of 40 nm selenium nanoparticles. (A) and (C) Unheated precursor selenium nanoparticles. (B) and (D) Precursor selenium nanoparticle solution after heating at 90°C for one hour.

Note: The bar in A and B represents 170 nm, and in C and D represents 80 nm.