Schematic diagram of the process flow: (a) SAM formation upon immersion in an ethanolic solution of HDT; (b) photothermal laser processing of the HDT SAM at λ = 532 nm; and (c) pattern transfer into the Au film upon etching in an aqueous solution of K2S2O3 and K3Fe(CN)6. Adapted from [11].