Skip to main content
. 2012 Mar 12;2012:397813. doi: 10.1155/2012/397813

Figure 3.

Figure 3

Oligonucleotide coating stability. Polypropylene sheets were coated with diX AM and oligonucleotides were applied to the coated surface. Oligonucleotides were detected by an ELISA system. Samples were exposed to a constant fluid flow inducing at least 9, 5 N/m2 shear stress on the surface for 1 h (n = 6).