Table 2.
Polymer | Coating Method | Film Thickness | Detection Limit | Reference |
---|---|---|---|---|
Ethylene-propylene copolymer | Drop cast followed by heating at 150°C | 4.2 μm | 80 ppb | [20] |
Poly(acrylonitrile-co-butadiene) | Spin coated | 5.1 μm | 10 ppb | [29] |
Teflon | Spin coated | 5.1 μm | 27 ppb | [16,29] |
Polyisobutylene | Drop cast | NA | 337 ppb | [30] |
NA = not available