. 2010 Oct;89(10):1057–1062. doi: 10.1177/0022034510375289

Figure 2.

Figure 2.

Surface view of single-cycle sliding damage in (a) porcelain fused to zirconia at Pn = 120 N; (b) graded G/Z/G at Pn = 2000 N; (c,d) monolithic zirconia at Pn = 600 N and 1000 N, respectively. Note two faint incomplete ring cracks indicated by solid arrows in (c). Sliding direction from left to right of micrographs.