Published in final edited form as: Chem Commun (Camb). 2011 Oct 6;47(43):11861–11863. doi: 10.1039/c1cc15002b

Fig. 1.

Fig. 1

(a) Diagram showing layer by layer assembly of (polymer I/GOx)2 films at graphite electrode. CVs of (polymer I/GOx)1 (grey) and (polymer I/GOx)2 (black) films in 0.1 M potassium phosphate buffer containing 0.15 M NaCl at 37 °C, pH 7.4 in (b) absence and (c) presence of 0.1 M glucose. Scan rate 5 mVs−1.