Table 1.
Sample | Mn (kDa)a | Mw (kDa)a | PDI (Mw/Mn) | Degreeb Branching |
Relative wt% PEGc |
---|---|---|---|---|---|
p(TETA/CBA) | 21.7 | 33.4 | 1.54 | 0.79 | - |
p(TETA/CBA)-PEG (TCP) | 24.5 | 31 | 1.27 | 0.87 | 4.0 |
Number average molecular weight (Mn), weight average molecular weight (Mw), and polydispersity (Mw/Mn) determined using FPLC.
Degree branching was determined by reduction of disulfide bonds with TCEP followed by the protection of free sulfhydryls with NEM and analyzed by MALDI-TOF.
NMR was used to estimate the relative wt% PEG by integrating p(TETA/CBA) and p(TETA/CBA/PEG) peak area under the curve (AUC).