Figure 1. Fabrication of iron oxide ribbons.

Figure 1

It includes (1) and (2) controllable nucleation and growth of the iron glycolate onto the surface of the reduced graphene oxide at 170°C, and (3) thermal annealing at different temperatures (250–400°C) in air.