. 2011 Jul 19;5(3):034102–034102-12. doi: 10.1063/1.3608138

Figure 4.

Figure 4

Effects of pH and molecular weight of PEI on layer thickness after 10 min incubation. In total, five polyelectrolyte layers were generated on planar (a) silanized with (3-glycidoxypropyl)trimethoxy silane and (b) non-silanized silicon surfaces using PEI with HMW = 750 kDa or LMW = 1.2 kDa.