Table 4.
Study | Grist-blasted cups % of mechanical fixation failures | Porous-coated cups % of mechanical fixation failures | Mean followup (years) or intervals of followup |
---|---|---|---|
Reikeras and Gunderson [28] | 25% | 7–10 | |
Lai et al. [16] | 38% | 10 | |
Miyakawa et al. [24] | 31% | 11–14 | |
Kim et al. [15] | 14% | 7 | |
Malchau et al. [20] | 18% | 6 | |
Bohm and Bosche [3] | 0% | 11 | |
Manley et al. [21] | 11% | 2% | 7.9 |
D’Lima et al. [7] | 6% | 6 | |
Bojescul et al. [4] | 17% | 15 | |
Engh et al. [11] | 0,4% | 7–15 | |
Garavaglia et al. [13] | 0% | 10 | |
Vicente et al. [29] | 12.3% | 11.4% | 10–12 |
Current study | 3.7% | 1% | 7.7 |