Published in final edited form as: J Biomed Mater Res A. 2012 May 24;100(8):2204–2210. doi: 10.1002/jbm.a.34119

Figure 5.

Figure 5

Representative epifluorescent images of EC actin filaments after 24h shear stress on FN (A) and RGD FSP (B) coated ePTFE grafts. Arrow indicates direction of shear stress. 86% of cells on RGD FSP coated grafts aligned within ±20° of the direction of flow, while only 53% of cells on FN were aligned.