Figure 6.

Figure 6

SEM of the inner surface of cell seeded PA tubes after 12 days in culture. (A) Aligned tube shows that SMCs migrated to the surface and organized with elongated features parallel for nanofiber alignment. (B) The non-aligned sample did not display much organization of SMCs.