. 2012 Jun 15;13(6):7393–7423. doi: 10.3390/ijms13067393

Figure 9.

Figure 9

TEM image of as-deposited ZnO/LSMO composite nanorod: (a) and (b) bright field, (c) and (d) dark field. (a) and (c) correspond to as-deposited ZnO/LSMO, (b) and (d) correspond to annealed ZnO/LSMO. The insets in (a) and (b) show the corresponding electron diffraction pattern. The insets in (c) and (d) show the corresponding EDS spectrum.