Skip to main content
. 2012 Feb;286(9):30–40. doi: 10.1016/j.jcat.2011.10.013

Table 6.

Effect of catalyst recycling on BET surface area, total pore volume, and average pore diameter.

Entry BET (m2/g) Total pore volume (cm3/g) Average pore diameter (Å)
MPSG 365 0.41 45
Pd(OAc)2-BOX-MPSG 192 0.23 47
Pd(OAc)2-BOX-MPSG after 1st use 112 0.15 55