Skip to main content
. Author manuscript; available in PMC: 2013 Sep 1.
Published in final edited form as: Acta Biomater. 2012 May 22;8(9):3436–3445. doi: 10.1016/j.actbio.2012.05.016

Figure 7.

Figure 7

SEM micrographs of the porosity in CPC scaffold. (A) After the dissolution of mannitol porogen by immersion for 1 d, macropores in CPC were created in the shapes of the entrapped mannitol particles. (B) Examples of pore interconnection, with arrows indicating the open connections in the bottom of a macropore. The macropore size in CPC ranged from approximately 50 to 343 µm, with an average of 218 µm.