Figure 2.

Figure 2

Film thickness vs. time for various concentrations of glucose in the core hydrogel. The conditions used were: 3.1µM GOx, 0.25mM Fe2+, 0.005wt% rhodamine-B acrylate, 10 mM MES pH 4.5 and 15wt% PEGDA575