Hydrogen peroxide concentration released into the bulk vs. time when the coated hydrogel construct is immersed in water just after the coating process (○) or after allowing the hydrogel to stand in a 0.05 mM Fe2+ solution for 15 min (Δ). The coating was 600 µm thick