Table 2 . Mechanical properties of cementomimetic layer as measured by nanoindentation (n=20 indentations) .
Layer | Er/GPa | H/GPa |
---|---|---|
Cementomimetic layer | 19±7 | 0.7±0.5 |
Native cementum | 15±4 | 0.8±0.3 |
Mineralized dentin | 26±3 | 1.0±0.2 |
Demineralized dentin | 5±3 | 0.2±0.2 |
Er, Young's modulus; H, hardness.