Skip to main content
. 2012 Aug 8;2012:281384. doi: 10.1155/2012/281384

Table 2.

Effect of various treatments on the physical properties of ramie fibre.

Type of treatment given to the fibre Stress at peak
(MPa)
Young's modulus
(GPa)
Strain at max. load
(%)
Brightness
(l)
Redness
(a)
Yellowness
(b)
Raw fibre (Control) 488.94 23.40 8.571 108.25 1.48 8.55
Chemical (12% NaOH) 478.73 26.06 6.78 121 0.91 3.42
Commercial fibre 374.1 13.69 13.21 115 1.03 4.75
Enzyme + NaOH (0.04%) 848.6 25.89 9.93 118.87 0.98 4.02