Cyclic voltammograms of χsol = 0.3 azidoundecanthiol (1) mixed monolayers taken after immersion in aqueous ethanol with catalyst and FcCOCCH (3) for 0 h (solid), 1 h (dashed), and 3 h (dotted). Scans were done in 1 M HClO4 with a scanning rate of 0.3 V/s. Potentials are measured relative to a Ag/AgCl/1 M KCl reference electrode