Skip to main content
. 2012 Jul 12;7(1):388. doi: 10.1186/1556-276X-7-388

Figure 3.

Figure 3

Change in T-NT diameter with anodization potential after 1 h anodization. The gap between electrodes was 2 cm. Insets show SEM micrographs of T-NT formed by anodization at 10, 30, and 50 V.