Amphotericin B ALBC literature

Study Elution Compression
Kweon et al. [7] Amphotericin B release is small but measurable
Mt very low, < 1% of amphotericin B load
Amphotericin B increased strength of 200 mg deoxycholate ALBC by 10%
Added poragen caused loss of strength over time in elution
Sealy et al. [10] Amphotericin B is released from 352 mg deoxycholate ALBC beads
Mt not reported
Not investigated
Goss et al. [4] Amphotericin B is not released from 200 mg deoxycholate ALBC Amphotericin B increases compressive strength of cement by 25%
Marra et al. [8] Case report
187.5 mg deoxycholate ALBC beads produce measurable amphotericin B levels in wound fluid