Skip to main content
. 2012 May 30;7(1):272. doi: 10.1186/1556-276X-7-272

Figure 6.

Figure 6

TEM BFI and SAED pattern of tenorite in PLA sample after prolonged dwelling in water. Note the slightly preferred orientation of the assembled tenorite nanoparticles in region I to show the (002) and {111} diffraction arcs. The sample was dwelled in water for 20 days after PLA treatment. The Ni counts are from the sample supporting the nickel grid.