Skip to main content
. 2012 Jul 12;10:29. doi: 10.1186/1477-3155-10-29

Figure 3.

Figure 3

X-ray diffraction patterns with (hkl) values of as-grown ZnO nanoparticles by sol–gel method, where folic acid concentration (weight/volume) has been (a) 0%, (b) 0.5%, (c) 1.3%, (d) 4.8%.