Table 4.

TiO2 Dye PPF Scaffold Accuracy – 2-Plate Test Scaffold Diameter Measurements*

Sample
Number
Plate 1
Diameter
(mm)
Plate 2
Diameter
(mm)
1 5.90 N/A**
2 6.02 5.83
3 5.93 5.92
4 5.97 5.84

Mean 5.92
Std Dev 0.07
*

Four 2-plate test scaffolds were rendered using a 150 s exposure time and a 200 mW/dm2 irradiance. The resin used for these samples contained a 2:1 PPF/DEF ratio with 2 wt% BAPO and 1 wt% TiO2. For each test scaffold, the diameter of each plate was measured using digital calipers. The expected diameter was 6.0 mm. The observed error is approximately 2 times the Perfactory device’s tolerance of 35 microns.

**

This plate rendered well but was damaged during post-processing.