Skip to main content
. 2012 Nov;295(2-3):186–194. doi: 10.1016/j.jcat.2012.08.008

Fig. 9.

Fig. 9

Pd3d5/2, In3d5/2, and VB regions on the initial In2O3-on-Pd “inverse catalyst” showing the transition from the initial oxide-on-metal state to the intermetallic InPd state in the temperature region around 523 K under MSR conditions.