Table 1.

Amounts of polyelectrolytes needed to compensate (zero) or completely reverse surface charge of nanoparticles, mg/mg PTX

Coating
step
Layer PLB16-5 PLL
zero recharged zero recharged
1 PLB on AOT 0.05 0.26 0.08 0.26
2 Hep on AOT/PLB 0.08 0.27 0.23 0.35
3 PLB on AOT/PLB/Hep 0.11 0.26 - -
4 Hep on AOT/(PLB/Hep)1.5 0.14 0.27 - -