Fig. 1.

Fig. 1

Scanning electron micrographs of RIF-free (a: 557 ± 399 nm), 10% RIF (b: 402 ± 225 nm), and 20% RIF (c: 665 ± 409 nm) PCL nanofiber scaffolds. d Scaffold fiber diameters for the control and RIF-encapsulated scaffolds are represented as mean ± standard deviation