Percentual change Δd = 100·(dwet-dorig)/dorig of the average particle diameter in aqueous environment dwet compared to the particle diameter without any water treatment dorig. Values are based on the statistics acquired from the SEM micrographs.

T = 20 °C T = 40 °C
Sample code Δd, 1 min Δd, 4 h Δd, 1 min Δd, 4 h
PN77.118K 6 ± 5 18 ± 5 -1 ± 5 6 ± 4
PN61.106K 51 ± 4 72 ± 5 2 ± 3 -16 ± 2
PN43.65K -1 ± 2 -21 ± 2 10 ± 3 2 ± 3